Dental glass ceramics, main ingredients are Lithium Disilicate, through special process. The average biaxial bending strength after complete crystallization is 637.3Mpa,TOP bending strength 670Mpa ,, which has passed FDA certification and product inspection and is higher than the standard strength value specified in ISO6892:2008 Dental Ceramics.

Dental glass ceramics, main ingredients are Lithium Disilicate, through special process. The average biaxial bending strength after complete crystallization is 637.3Mpa,TOP bending strength 670Mpa ,, which has passed FDA certification and product inspection and is higher than the standard strength value specified in ISO6892:2008 Dental Ceramics.